Blisk
Before
| Tool |
Grindstone |
|---|---|
| Problem |
It took time for deburring due to the complicated design of workpiece. Resulted in unstable edge quality. |
After
| Tool | XEBEC Brush Surface (A21-CB25M) |
|---|---|
| Result | By the introduction of automated deburring, 1 operator can operate the multiple machining centers. |
Workpiece information

| Industry |
Aerospace |
|---|---|
| Part name |
Blisk |
| Material type |
Inconel |
| Cutting process |
Ball end mill processing |
Processing conditions
| Tool |
XEBEC Brush Surface (A21-CB25M) |
|---|---|
| Details of processing |
Deburring after ball-end milling process |
| Spindle speed (min⁻¹) |
4,000 |
| Table feed (mm/min) |
2,400 |
| Depth of cut (mm) |
0.5 |
| Machining time (sec) |
– |