Connecting rod (Edge face)
Before
| Tool |
Wire brush |
|---|---|
| Problem |
Burrs remained. Brushes deformed and caused the quality control problem in mass production. |
After
| Tool | XEBEC Brush for Surface (A31-CB25M) |
|---|---|
| Result | Automated deburring with stable quality during production realized. |
Workpiece information

| Industry |
Automotive |
|---|---|
| Part name |
Connecting rod (edge face) |
| Material type |
S45C |
| Machining process |
Front cutter processing |
Processing conditions
| Tool |
XEBEC Brush for Surface (A31-CB25M) |
|---|---|
| Details of processing |
Deburring the edge face after milling process |
| Spindle speed (min⁻¹) |
4,000 |
| Table feed (mm/min) |
2,500 |
| Depth of cut (mm) |
1 |
| Machining time (sec) |
– |