Cooling fin
Before

| Tool |
Wire brush |
|---|---|
| Problem |
After deburring process, burrs remained due to complicated shape of workpiece. |
Workpiece information

| Industry |
Automotive |
|---|---|
| Part name |
Cooling fin |
| Material type |
Aluminum alloy |
| Machining process |
Others |
Processing conditions
| Tool |
XEBEC Brush for Surface (A11-CB40M) |
|---|---|
| Details of processing |
Deburring the edge after cutting process |
| Spindle speed (min⁻¹) |
3000 |
| Table feed (mm/min) |
800 |
| Depth of cut (mm) |
1 |
| Machining time (sec) |
– |