Crankshaft (Cross hole)
Before
| Tool |
Cutter |
|---|---|
| Problem |
Burrs left by manual deburring. Caused low production rate. |
After
| Tool | XEBEC Stone Flexible Shaft (CH-PM-5R-C01) |
|---|---|
| Result | By introduction of automated deburring with machining center, stable edge quality and cost reduction realized. |
Workpiece information

| Industry |
Automotive |
|---|---|
| Part name |
Crankshaft (Cross hole) |
| Material type |
S48C |
| Machining process |
Drilling |
Processing conditions
| Tool |
XEBEC Stone Flexible Shaft (CH-PM-5R-C01) |
|---|---|
| Details of processing |
Cross hole deburring after drilling process |
| Spindle speed (min⁻¹) |
1,350 |
| Table feed (mm/min) |
– |
| Depth of cut (mm) |
0.5 |
| Machining time (sec) |
– |