Input shaft (Cross hole)
Before
| Tool |
Abrasive-impregnated nylon brush |
|---|---|
| Problem |
Burrs are left by manual deburring. It caused low efficiency in processing. |
After
| Tool | XEBEC Brush for Cross hole (CH-A12-5M + CH-A12-7M) |
|---|---|
| Result | Full automation realized with custom made machine. No burrs left and finish quality improved. |
Workpiece information

| Industry |
Automotive |
|---|---|
| Part name |
Input shaft (Cross hole) |
| Material type |
SCM |
| Machining process |
Drilling |
Processing conditions
| Tool |
XEBEC Brush™ Crosshole (CH-A12-5M + CH-A12-7M) |
|---|---|
| Details of processing |
Crosshole deburring after drilling process |
| Spindle speed (min⁻¹) |
9000 |
| Table feed (mm/min) |
300 |
| Depth of cut (mm) |
– |
| Machining time (sec) |
– |