Reduction gear (Cross hole)
Before
| Tool | Wire brush |
|---|---|
| Problem | Burr remained by low grinding power. Quality unstable due to deformation of brush material. |
After
| Tool | XEBEC Brush Crosshole (CH-A12-3L) |
|---|---|
| Result | Burr eliminated and stable quality realized at mass-production line. |
Workpiece information
| Industry | Automotive |
|---|---|
| Part name | Reduction gear (Cross hole) |
| Material type | Scr420 |
| Machining process | Drilling |
Processing conditions
| Tool |
XEBEC Brush Crosshole (CH-A12-3L) |
|---|---|
| Details of processing |
Cross hole deburring after drilling process |
| Spindle speed (min⁻¹) |
10,800 |
| Table feed (mm/min) |
300 |
| Depth of cut (mm) |
– |
| Machining time (sec) |
– |