Yoke
Before

| Tool |
Cutter, sandpaper |
|---|---|
| Problem |
Manual deburring caused unstable quality and high labor cost. |
After

| Tool |
XEBEC Brush for Surface (A31-CB25M) |
|---|---|
| Result |
Fully automated deburring enabled stable quality and shorter processing time. Also the efficiency of processing improved by changing the burr direction by review of pre-process. |
Workpiece information

| Industry |
Automotive |
|---|---|
| Part name |
Yoke |
| Material type |
SUS430 |
| Machining process |
Chamfering |
Processing conditions
| Tool |
XEBEC Brush for Surface (A31-CB25M) |
|---|---|
| Details of processing |
Deburring the section after chamfering process |
| Rotation speed (min-1) |
3,000 |
| Feed rate (mm/min) |
– |
| Depth of cut (mm) |
1 |
| Machining time (sec) |
– |